#1 |
Member
Join Date: Dec 2004
Location: Witness Protection Program
Posts: 1,730
|
![]()
i've tried industrial acetone, and steam (if it was indeed cosmoline). and it's too uniformed to have been FECL, unless the owner removed the asang and handle, then re sharpened the edges all the way to the katik. i will try denatured alcohol.
|
![]() |
![]() |
![]() |
#2 |
EAAF Staff
Join Date: Dec 2004
Location: Louisville, KY
Posts: 7,280
|
![]()
IF it was nickeled (once used for anti-rust and to make blades shiny) then it will take more than denatured alcohol.
![]() ![]() |
![]() |
![]() |
![]() |
#3 |
Member
Join Date: Dec 2004
Location: Witness Protection Program
Posts: 1,730
|
![]()
doubt if it's nickeled. i worked on a barung this past summer that was nickel plated. yup, it was a female dog! used muriatic acid and still took me a good couple hours...
|
![]() |
![]() |
![]() |
|
|