Hello Kerislovers,

the animals on top of the ganja are not original but made recently. The blade itself is not a good one because of the low condition. Remember Balinese Blades are polished not etched like the Javanese. Etching of Balinese blades came up maybe in the 70ties because of the lack of caretaking. To get a Balinese keris in good first class condition is almost impossibleSee: Hamzuri 1982-83 Petunjuk Singkat Tentang Keris p. 8.

Animals on Balinese blades (ganja) are sometimes present even of gold and sometimes like the Javanese Singa Barong (not a tiger), Gajah, winged horse and so on. impossible.
See: Hamzuri 1982-83 Petunjuk Singkat Tentang Keris p. 8.

Its said the meaning of this animals is a date and also like a medal of honour for bravery especially under Sultan Agung.

empu kumis
empu kumis is offline   Reply With Quote
Old 13th March 2005, 10:25 PM   #2
capt.smash
Member
 
Join Date: Jan 2005
Location: Devon ,England
Posts: 80
Default

Thanks Henk for looking that up thats a great help and interesting

Hi Empu Kumis thanks for your comments this blade is highly polished and you cant feel the pamor if you run your finger over it but does have random pitting and wear from past corrosion im very sure its older than the 1970,s .

Also after more cleaning i have discovred that there is a wafer thin gold shim between the blade and the ganja its only visable in a couple of places and is incredibly thin my camera wont zoom in close enough to catch it properly... strange but interesting

Last edited by capt.smash; 14th March 2005 at 12:06 AM.
capt.smash is offline   Reply With Quote
Old 14th March 2005, 09:01 PM   #3
empu kumis
Member
 
empu kumis's Avatar
 
Join Date: Dec 2004
Location: Germany
Posts: 17
Default

Hello Capt. Smash,

its not only the corrosion but also the incomplete greneng and the blade is to narrow. It could be reshaped. This has been done many times to rise the prices in Bali and even more in Jawa.

The blade itself is older but reshaped. Up to now there has been almost no research about the age of Balinese kerisses. If somebody telling you the age of a Balinese keris its always pure speculation. Even to tell about where it comes from (Southbali or Northbali) is difficult and in Bali almost everythings is forgotten.

Last edited by empu kumis; 14th March 2005 at 09:12 PM.
empu kumis is offline   Reply With Quote
Old 17th March 2005, 01:10 PM   #4
capt.smash
Member
 
Join Date: Jan 2005
Location: Devon ,England
Posts: 80
Default

After some TLC and a visit to doctor arsenic....nice pamor in my opinion
Attached Images
    

Last edited by capt.smash; 17th March 2005 at 03:33 PM.
capt.smash is offline   Reply With Quote
Old 17th March 2005, 05:53 PM   #5
Henk
Member
 
Henk's Avatar
 
Join Date: Dec 2004
Location: The Netherlands
Posts: 1,209
Default

Did you that by yourself??? The result is great !!! Next step is restoring the gold part and if possible a good dress for this fellow.
Henk is offline   Reply With Quote
Old 17th March 2005, 05:59 PM   #6
Bill
Member
 
Join Date: Feb 2005
Location: Chicago area
Posts: 327
Default

Looks very good Captain, as some of your past posts show questions about etching, tell us about your experiances to date.
Bill is offline   Reply With Quote
Old 17th March 2005, 07:20 PM   #7
capt.smash
Member
 
Join Date: Jan 2005
Location: Devon ,England
Posts: 80
Default

HI guys, Henk yes i did it myself i am currently looking at gold leaf/gilding and have found that gold leaf is quite cheep so i will be doing this very soon .Im also looking into re-doing the fadeing an in some places worn away engraveing on the blade but this is a long term project[i already have the engraveing tools but it will require some further experimentation before hand].


Hi Bill i have been building up to this kind of project for some time and just as i was ready this blade fell into my lap as if it was meant to be .My first task was the staining solution witch as i described in my thread on "warangan".Firstly i had to find a source of Arsenic witch as you know is a banned substance in most countries and after some searching and help from other members i found that warangan[the traditional mineral for staining keris] was probably the ore Realgar[Arsenic sulfide]easily sourced on ebay then powdering it[ a lump of ore about an inch square part crystal part rock]and adding it to about 1 and a half liters of grapefruit juice.I tested this on an inferior trade blade that i got for this task and it worked well although i have found the grapefruit juice is only mildly acidic and only removes dirt and dosent etch the blade [ideal for a bali blade that has a polished surface] so for a more acidic solution i will use limes.I soaked the blade for 1 and a half days in my bathroom with ambient temprature of about 20deg C [slow but easily controllable].

The hardest part was prapareing/restoreing the blade.As you can see from the pics it was in bad shape with lots of corosion, rust ,scratches and pitting along the blade[the pamor not visable in a few plces], fortunately most of the pitting was only very shallow and i spent a day and a half of intermitant sanding with 6 grades of sandpaper [the type used in praparing car bodywork] starting with p100 to remove the surface material on both sides to a point where the pittingwas minimal and i could put a polish on the blade[aproximately quarter of a milimeter off both sides but im guessing there]this was the hardest part becuase i had to draw a line between a good surface and changeing the shape /lines of the blade witch i didnt want to do.After this i then gradualy went down in courseness of sandpaper p180,p320,p400,p800,p1500 till it was in a position to be easily polished.
Some of our more traditional keris lovers may want to look away now I then did a quick pass on a rotary buffing wheel to polish the blade to a nice shine.And finaly gave the blade a few whipes with a rag soaked in sulfuric acid[car battery acid] to re-open the grain of the blade so the pamor could be set free.
In all i probaly removed about 3 quarters of a mill,s worth of material from the blade ,amazeing the difrence it has made and with no detremental afects on the strength of the blade.

Make what you will of it,any coments welcome

sorry about the grammar
Attached Images
 

Last edited by capt.smash; 17th March 2005 at 08:08 PM.
capt.smash is offline   Reply With Quote
Reply


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +1. The time now is 07:42 AM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2025, vBulletin Solutions Inc.
Posts are regarded as being copyrighted by their authors and the act of posting material is deemed to be a granting of an irrevocable nonexclusive license for display here.