By the way, the iron beneath the gold on the first sword, seems to have deteriorated a little and gold is becoming lose. Any ideas on how to fix this, without making a long term mess, as happens with old varnish.
|
![]() |
![]() |
![]() |
#2 |
Member
Join Date: Jun 2005
Location: England, Northumberland
Posts: 85
|
![]()
It has been suggested by a friend that I may try using a PVA mix, such as Unibond that dries clear. Any suggestions to that? "Like oh my god no!!! Dont do that"
I need advice people, please ![]() Cheers Andy |
![]() |
![]() |
![]() |
#3 |
Member
Join Date: Dec 2004
Location: What is still UK
Posts: 5,887
|
![]()
Andy, PVA is good as it drys clear and if reversible being water soluble. Any hamfisted work can be soaked and no damage done, a little more tricky with fabrics and other very delicate things. Tim
|
![]() |
![]() |
![]() |
#4 |
Member
Join Date: Dec 2004
Location: Greensboro, NC
Posts: 1,089
|
![]()
It is a difficult thing to combat when the hilt is as profusely koftgari'ed as the example you post. When the base metal begins to rust, you risk either sealing in moisture if you attempt to do that to preserve which could cause further rusting and any attempts to do anything else could remove more of the goldwork. Your best bet is to keep the hilt dry and in low humidity going forward to maintain it.
|
![]() |
![]() |
![]() |
|
|