Ethnographic Arms & Armour
 

Go Back   Ethnographic Arms & Armour > Discussion Forums > Ethnographic Weapons
FAQ Calendar Today's Posts Search

Reply
 
Thread Tools Search this Thread Display Modes
Old 6th February 2005, 05:31 AM   #1
rasdan
Member
 
rasdan's Avatar
 
Join Date: Dec 2004
Location: Kuala Lumpur
Posts: 369
Default

Hi Capt,

From what i know, warangan is realgar. And yours looks much better with a higher arscenic sulphate content. Unfortunately i havent had the oportunity to use neither since arscenic is a controlled mineral in Malaysia. Perhaps others had experience.
rasdan is offline   Reply With Quote
Old 6th February 2005, 10:58 AM   #2
capt.smash
Member
 
Join Date: Jan 2005
Location: Devon ,England
Posts: 80
Default

Hi Rasdan thanks that was the info i was after...incidentaly i have looked into Realgar and aparently it is an unstable mineral it eventualy alters to a diffrent mineral called pararealgar and after that to powder[it is recomended to keep it in the dark and out of direct sunlight as this causes the colour to fade]...i wonder if the specimen you had was mined and stored long enough for it to alter and lose some of its colour...i have no ideah if this afects the arsenic content or mabe im thinking that mabe they let it alter on purpose as this would make it easier to crush and powder.
Anyway im going to order some and give it a try and ill post my results.
smashy
capt.smash is offline   Reply With Quote
Old 15th March 2005, 02:19 PM   #3
capt.smash
Member
 
Join Date: Jan 2005
Location: Devon ,England
Posts: 80
Default

HI guys i thaught id update this thread.After some experimentation i have discovred that Realgar [Arsenic sulfide] works very well once powdred[it crushes easily] and added with most citrus juice[i used grapefruit juice & also tried pineapple ]realgar is easily sourced as a mineral[ebay] so now everyone has the chance to have some fun and can have a go if they wish . [BUT BE CAREFUL THIS IS POISON AFTER ALL]

I also tried orpiment[arsenic trisulfide]but found it hard to powder and didnt work as well.
Attached Images
 
capt.smash is offline   Reply With Quote
Old 19th March 2005, 11:01 PM   #4
BSMStar
Member
 
BSMStar's Avatar
 
Join Date: Jan 2005
Location: Kansas City, MO USA
Posts: 312
Default Something else to consider....

Hi Captain!

Something I tried a long number of years ago on silver (to artificially "oxidize" it), is Liver of Sulfur (Potassium Sulfide). I have not tried it with iron (yet), but since it is chemical similar to Arsenic sulfide and leaves a black "stained" surface, it just might do the trick.

It is more readily available than Arsenic sulfide, and safer to work with too (but use plenty of ventilation), it just may be a good substitute. Buy it in dry form, mix about one to two teaspoons to one pint of hot water, and use within 48 hours. It will lose strength over time (that is the rotten eggs you smell as the sulfur leaves).

Let me know if you need more info. I would be interested in the results of any experiments made with this sulfide solution. I may work better in mild acid solution like lime juice...

Best regards,

BSMStar
BSMStar is offline   Reply With Quote
Reply


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +1. The time now is 09:24 PM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2025, vBulletin Solutions Inc.
Posts are regarded as being copyrighted by their authors and the act of posting material is deemed to be a granting of an irrevocable nonexclusive license for display here.