Default

Detlef, I use mostly silver solder when working with brass or copper though on some occasions I will still use lead solder with a rosin flux, I never use an acid base flux on anything brass or copper when doing repair work. All the bands I made and used on this gunong are silver soldered for strength and durability.

Best,
Robert
Robert is offline   Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +1. The time now is 02:27 AM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2025, vBulletin Solutions Inc.
Posts are regarded as being copyrighted by their authors and the act of posting material is deemed to be a granting of an irrevocable nonexclusive license for display here.