Brian: Instead of using ferric chloride, you might want to try phosphoric acid. It is sold by Orchard Supply Hardware under the name "metal etch" I have used it for many years to etch layer welded blades, especially moro swords. I think it gives a much better look to the steel, a silver and black look. I used ferric on wootz until just recently. I tried phosphoric on a wootz piece and the results were outstanding. Instead of diluting it ,use it right out of the bottle as i have found it really dosen't need to be diluted. It also helps if the blade is warmed with a propane torch. Just warm enough so you can't hold your hand on it. It makes the high carbon areas stand out better. Ferric chloride always seems to give a gray-green etch which i dont think looks as good as a phosphoric etch. I also have never had a problem with using straight tap water. Possibly my area of the country (Central Calif) might have different or less dissolved minerals than where Bill lives (Atlanta). That might make a big difference in the kook of the final etch.....Dave
DaveS is offline   Reply With Quote
 

Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +1. The time now is 12:25 AM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2025, vBulletin Solutions Inc.
Posts are regarded as being copyrighted by their authors and the act of posting material is deemed to be a granting of an irrevocable nonexclusive license for display here.