6th September 2008, 01:54 AM | #31 | |
Member
Join Date: Apr 2005
Posts: 3,254
|
Hello Ron,
Quote:
I've also heard the suggestion that this may have been done with blades where not enough material was left for forming a tang during the original forging. I don't think so: obviously the skill of the bladesmiths was high. Even if your pieces for the sandwich construction were not large enough for a tang, the easiest and stronger solution would still be to take an additional suitable piece of mild steel and weld it between the layers during the sandwich step... Regards, Kai |
|
|
|