I don't think there's really a set ratio as different steels react in different times and ways with fecl .
I always start out with 20% fecl or less .
I always mix only with distilled water .
You can always boost the ratio from there .

Just keep the solution moving on the blade surface .

The only piece I have let stand in a solution was a contemporary Indian kanjar with a bird's eye damascus pattern , I was looking to make a topographical etch and it worked in about 30 minutes .
Rick is offline   Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +1. The time now is 07:17 AM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2025, vBulletin Solutions Inc.
Posts are regarded as being copyrighted by their authors and the act of posting material is deemed to be a granting of an irrevocable nonexclusive license for display here.