Etching mixture
Hello ,
I recently go through the different threads regarding etching old blades and was very disappointed with the mixture I have prepared on a couple of old keris . I have prepared a mixture with lime juice ( 14 pealed before taking the juice ) and Trioxide arsenic lab quality( 1 tea spoon ) with enough water to get half liter of magic potion . 1 week rest with a piece of steel wool ... and then a go for a test with plenty of sun light . Could some " experts " give me the right proportion to use : lime juice + Trioxide arsenic + water (?) to make 1 litre . Thanking you in advance for your help Henri |
|
|