Old 7th March 2016, 03:39 PM   #1
mariusgmioc
Member
 
mariusgmioc's Avatar
 
Join Date: Sep 2014
Location: Austria
Posts: 1,903
Question Restauration of Pamor

Recently, I aquired a Wedhung with quite a spectacular pamor. Unfortunately, the blade had some spots of active rust that had to be removed. I managed to remove nicely all traces of active rust, but I also washed out most of the pamor as well. I am quite adept at etching wootz blades, but noticed to my surprised that my technique doesn't work with the pamor.
Does anybody know a where I can I have the pamor restored?
mariusgmioc is offline   Reply With Quote
Old 7th March 2016, 04:24 PM   #2
David
Keris forum moderator
 
David's Avatar
 
Join Date: Aug 2006
Location: Nova Scotia
Posts: 7,120
Default

The technique for staining blades is done with warangan (arsenic and lime). If you search the site you should find some instructions on this, though obtaining arsenic can be difficult for many. Some people use industrial grade arsenic which gives a fairly consistent result while many grind up the actual mineral for the process which can be less consistent, but might be easier to get your hands on.
There are people who do this as a service, but few outside of Indonesia. Where do you live?
David is offline   Reply With Quote
Old 7th March 2016, 05:52 PM   #3
mariusgmioc
Member
 
mariusgmioc's Avatar
 
Join Date: Sep 2014
Location: Austria
Posts: 1,903
Default

Quote:
Originally Posted by David
The technique for staining blades is done with warangan (arsenic and lime). If you search the site you should find some instructions on this, though obtaining arsenic can be difficult for many. Some people use industrial grade arsenic which gives a fairly consistent result while many grind up the actual mineral for the process which can be less consistent, but might be easier to get your hands on.
There are people who do this as a service, but few outside of Indonesia. Where do you live?
Thank you very much for your reply!

I live in the Netherlands, and here only asking about arsenic can land you in hot water. So there is no way I can legally get it. However, I will travel next month to Indonesia, so if you know any place there would be quite helpful.
mariusgmioc is offline   Reply With Quote
Old 7th March 2016, 09:47 PM   #4
David
Keris forum moderator
 
David's Avatar
 
Join Date: Aug 2006
Location: Nova Scotia
Posts: 7,120
Default

There are an awful lot of keris collectors (and keris) in The Netherlands. Perhaps there is someone there who does traditional warangan treatments.
I cannot tell you much about who can do this for you in Indonesia. Perhaps others can help you there.
David is offline   Reply With Quote
Old 8th March 2016, 07:23 AM   #5
mariusgmioc
Member
 
mariusgmioc's Avatar
 
Join Date: Sep 2014
Location: Austria
Posts: 1,903
Default

Quote:
Originally Posted by David
There are an awful lot of keris collectors (and keris) in The Netherlands. Perhaps there is someone there who does traditional warangan treatments.
I cannot tell you much about who can do this for you in Indonesia. Perhaps others can help you there.
Thank you for trying!
I know a keris dealer here who might help.
In the worst case I will start experimenting myself with the chemicals I have.
mariusgmioc is offline   Reply With Quote
Old 8th March 2016, 03:58 PM   #6
David
Keris forum moderator
 
David's Avatar
 
Join Date: Aug 2006
Location: Nova Scotia
Posts: 7,120
Default

Quote:
Originally Posted by mariusgmioc
In the worst case I will start experimenting myself with the chemicals I have.
Well, as i state before, there is a bit of material in our archives on staining keris blades, including many suggestions on alternatives to using arsenic. Give a search and see what you find.
David is offline   Reply With Quote
Old 8th March 2016, 09:16 PM   #7
Rafngard
Member
 
Rafngard's Avatar
 
Join Date: Jun 2015
Location: Minneapolis,MN
Posts: 340
Default

Is anyone doing this in the U.S? I have a blade or two that could use an etch. I mentioned the possibility of trying this at home to my significant other, and her eyes got wide, and, well, let's just say I'm glad she didn't have a keris handy.

Thanks,
Leif
Rafngard is offline   Reply With Quote
Old 9th March 2016, 10:22 AM   #8
semar
Member
 
semar's Avatar
 
Join Date: Jul 2007
Posts: 272
Default warangan

hello depends ware you will go when you go to yogyakarta ik can help you with that i know 2 tukang maranggi

regards semar
semar is offline   Reply With Quote
Old 9th March 2016, 10:32 AM   #9
mariusgmioc
Member
 
mariusgmioc's Avatar
 
Join Date: Sep 2014
Location: Austria
Posts: 1,903
Default Thank you!

Quote:
Originally Posted by semar
hello depends ware you will go when you go to yogyakarta ik can help you with that i know 2 tukang maranggi

regards semar
Thank you for your assitance!

Yes, I will go to Yogyakarta in May and I can take the Wedhung with me to have it etched.

So, any more information will be welcomed!

Best regards,

Marius
mariusgmioc is offline   Reply With Quote
Old 9th March 2016, 12:30 PM   #10
ariel
Member
 
ariel's Avatar
 
Join Date: Dec 2004
Location: Ann Arbor, MI
Posts: 5,503
Default

Quote:
Originally Posted by Rafngard
Is anyone doing this in the U.S? I have a blade or two that could use an etch. I mentioned the possibility of trying this at home to my significant other, and her eyes got wide, and, well, let's just say I'm glad she didn't have a keris handy.

Thanks,
Leif
Buy Selenium Dioxide on Amazon. Cheap, reliable, safe, perfect blueing for guns and knives.
ariel is offline   Reply With Quote
Old 9th March 2016, 03:29 PM   #11
David
Keris forum moderator
 
David's Avatar
 
Join Date: Aug 2006
Location: Nova Scotia
Posts: 7,120
Default

Quote:
Originally Posted by ariel
Buy Selenium Dioxide on Amazon. Cheap, reliable, safe, perfect blueing for guns and knives.
Ariel is no doubt correct that Selenium Dioxide will raise the pamor on your blade. It won't give you the correct traditional coloring that arsenic will render. So in the end it all depends on your preferences and how authentic you want your blade to look in the end.
David is offline   Reply With Quote
Old 9th March 2016, 05:00 PM   #12
mariusgmioc
Member
 
mariusgmioc's Avatar
 
Join Date: Sep 2014
Location: Austria
Posts: 1,903
Default Thank you but...

... it doesn't work!

I already tried it and yes, I can get a very nice black blade but no pamor visible. I also tried different concentrations but still the results are quite dissapointing. I also tried Nital and Ferric Chloride that I normally use for etching wootz blades, but with pathetic results. So, what works for etching wootz or blacking steel, apparently doesn't work for revealing the pamor... or at least I didn't know how to make it work.

PS: Selenium dioxide in diluted form works also fine for revealing the watering pattern of wootz.
mariusgmioc is offline   Reply With Quote
Old 13th March 2016, 01:31 AM   #13
ariel
Member
 
ariel's Avatar
 
Join Date: Dec 2004
Location: Ann Arbor, MI
Posts: 5,503
Default

That's interesting! How much do you dilute it?
ariel is offline   Reply With Quote
Old 13th March 2016, 03:42 AM   #14
semar
Member
 
semar's Avatar
 
Join Date: Jul 2007
Posts: 272
Default

hello Marius with date you are in Djogya en ware you stay

reagads semar
semar is offline   Reply With Quote
Old 13th March 2016, 07:49 PM   #15
mariusgmioc
Member
 
mariusgmioc's Avatar
 
Join Date: Sep 2014
Location: Austria
Posts: 1,903
Default

Quote:
Originally Posted by ariel
That's interesting! How much do you dilute it?
I started from Perma Blue which is based on Selenium Dioxide and Nitric acid, which I already had diluted to about 20%. (At this concentration I etched an Indian Katar that I didn't manage to etch with the classic Nital and Ferric Chloride (even this concentration blackened the Katar completely but upon gentle wiping with Pre-lim, I got a very nice an visible watering wootz structure).) Then I diluted this even more to about 10%, but I only got a nice and uniform grey patina that didn't reveal the pamor even after selective cleaning with Pre-lim.

PS: I used undiluted Perma Blue for blacking an antique Japanese Tsuba with stellar results, and that's how I had it on hand to experiment with the Wedhung.
mariusgmioc is offline   Reply With Quote
Old 13th March 2016, 07:58 PM   #16
mariusgmioc
Member
 
mariusgmioc's Avatar
 
Join Date: Sep 2014
Location: Austria
Posts: 1,903
Default

Quote:
Originally Posted by semar
hello Marius with date you are in Djogya en ware you stay

reagads semar

Didn't finish my itinerary yet, but I will let you know.
mariusgmioc is offline   Reply With Quote
Reply

Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +1. The time now is 10:01 PM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2024, vBulletin Solutions Inc.
Posts are regarded as being copyrighted by their authors and the act of posting material is deemed to be a granting of an irrevocable nonexclusive license for display here.