14th June 2009, 06:54 PM | #1 |
(deceased)
Join Date: Dec 2004
Location: East Coast USA
Posts: 3,191
|
Wootz pattern popped!
I picked this jambiya up a couple of years ago but could not be sure if the blade was real wootz or acid etched faux wootz. I decided to sand and etch the blade with nice results.
|
14th June 2009, 07:46 PM | #2 |
Vikingsword Staff
Join Date: Nov 2004
Posts: 6,288
|
Nice Lew,
What did you use to bring it up ? |
14th June 2009, 08:13 PM | #3 |
(deceased)
Join Date: Dec 2004
Location: East Coast USA
Posts: 3,191
|
A fresh batch of ferric chloride and distilled water with a hot water rinse.
|
14th June 2009, 10:04 PM | #4 |
Vikingsword Staff
Join Date: Nov 2004
Posts: 6,288
|
Thanks Lew, duly noted .
Ratio of fecl to h2o ?? |
14th June 2009, 11:20 PM | #5 | |
(deceased)
Join Date: Dec 2004
Location: East Coast USA
Posts: 3,191
|
Quote:
|
|
14th June 2009, 11:24 PM | #6 |
Member
Join Date: Dec 2004
Location: Kernersville, NC, USA
Posts: 793
|
Sweet!