Hi again and happy new year.....
Sorry for the delay but i had a problem with my dsl connection and after that holidays came.
Dear A.G.Maisey i used limes for the supermarket.I follow the procedure that was posted in an other post.
Quote:
Basically, there would be 4 general steps for keris etching in traditional way.
1. Soak the blade in coconut water and lime juices solutions. This step only necessary when the blade is heavily corroded or having an old, stubborn etch. The soak would last usually from 1 night to 1 week, depending on the severity. This step should be omitted if we have a clean blade.
2. Mutih (from putih=white. Mutih=to make it clean white). An important step which directly affect your etching result. Pure lime juice is brushed on the blade, then wait a moment until it react with the blade (the color change to yellowish-green), then brush again. Continue brush-and-wait prosess, and add a small amount of juices only when necessary (e.g. when the blade dry-up). You should see the juices get thicken and turn into dark brown during the process. Wash the blade when the juices has became too dark or when the blade has been white-clean. Care should be taken to get rid all the juice/acid, or the rust would start to develop again as soon as the blade dry.
3. Marangi= to apply the warangan solution.
4. Oiling
I did everything except step 3 because i can't find arsenic.
I used half a lime.