Hi lemmythesmith,
A bit difficult to understand the strange position of this heat treatment ! No ?
Basically, I think you are right, the difference of colour is due to heat, but was it really a treatment to harden the metal or is it just an error ?
The forging is well done, look at the peksi, with its little hole and the heatwelding to the blade and the pamor, is not a simple one. I would love to be able to forge such a pamor .
I just do not understand that colour change.
Regards
Michel