Quote:
Verhoeven makes it clear that Fe3C (cementite) is crucial to forming the watering pattern. He also makes it clear that they can only form in the hypereutectoid state.
While it is true that excess cementite only shows up in hypereutectoid steels, I think Verhoeven might be mistaken in saying the cementite is crucial to the pattern.
This blade is 0.79%, measured at a lab -


This blade is somewhat less in carbon, but has not been lab analysed -



The patterns are not due to extra cementite; since they are below the eutectoid point the carbon is all wrapped up in pearlite.
Do the patterns look like sham wootz, or regular, or somewhere in between?

I think the ultimate answer is to get more blades checked at the lab, but we may find the old pattern-based distinctions are as much related to working methods as alloy.