View Single Post
Old 20th February 2011, 12:21 PM   #41
Atlantia
Member
 
Atlantia's Avatar
 
Join Date: Jun 2008
Location: The Sharp end
Posts: 2,928
Default

Quote:
Originally Posted by GIO
I also use warangan, but was told that somebody gets very good results with iron chloride (or iron sulphur ?). I Don't remember well, sorry. I have seen a couple of blades etched this way and the result was perfect.
Maybe other friends are better informed.


Hi Gio,

Iron Chloride would be a much safer option. Thanks for the info.
Best
Gene